Nickel Superalloy Powder – Ni625

Nickel Ni625 Metal Powder For Additive Manufacturing

HIGH-PERFORMANCE PARTS START WITH HIGH-QUALITY NICKEL METAL POWDER

6K Additive Ni625 metal powders for additive manufacturing. Ni625 is Ni-Cr-Mo-Nb solid solution superalloy with high corrosion resistance, high strength, excellent fatigue resistance, and high-temperature stability. Ni625 properties make this alloy application for additive manufacturing interesting for marine and nuclear applications where corrosion is a concern and aerospace and racing car applications where high-temperature stability is required. The poor machinability of Ni625 makes it ideal for additive manufacturing. Ni625 metal powder is available in various sizes for 3D metal additive manufacturing.

Ni625 metal powder is available in a variety of sizes. 6K Additive is a leading metal powder manufacturer, so we can customize the PSD that you are looking for.

6K-Premium-powders
Ni625 Metal Powder 3D Printed Impeller

3D Printed Impeller printed using 6K Additive spheroidized powder

6K Additive Nickel Ni625 Metal Powders

6K Inc UniMelt process is able to achieve industry-leading yields and obtain nickel Ni625 metal powders that perfectly match your desired particle size distribution (PSD) allowing for a variety of additive manufacturing processes when using nickel superalloy powder.

Ultra Clean
No Satellites
High Sphericity
Free Flowing
High Apparent Density
Low Porosity
Exceptional Lot-to-Lot Consistency
Conforms to AMS7006
Conforms to ASTM F3055
6K-inc-NICKEL-625-Superalloy-Powder

6K Additive Ni625 powder SEM

Industries & Applications for Nickel Ni625 Metal Powder

Ni625 powder is highly valued across a range of industries for its exceptional properties and versatile applications. With its outstanding properties, nickel metal Ni625 has gained significant popularity in additive manufacturing, allowing for the production of intricate components in a wide range of crucial AM industries such as:

Additive Manufacturing
Aerospace
Marine
Chemical Processing
Oil & Gas
Nuclear Power Sectors
6k-inc-NICKEL-625-am-Powder

6K Additive Ni625 powder SEM

Key Properties of Nickel Ni625 Metal Powder

Ni625 metal powders stands out for its impressive range of properties. With high-temperature strength as one of its defining features, this nickel metal powder remains robust even in extreme heat conditions. Additionally, it boasts superior corrosion resistance, making it highly reliable in various additive manufacturing corrosive environments.

High-Temperature Strength
Superior Corrosion Resistance
Precipitation Hardening
Excellent Fatigue Resistance
Wide Operating Temperature Range
imgi_5_6k-Nickel-Life-Cycle-Assessment

LCA Nickel Life Cycle Assessment Report

Foresight Management completes the first-ever LCA for AM powder manufacturing processes for nickel powder production.

Sustainably Produced Nickel Metal Powder

At 6K Additive, our nickel powders are sourced sustainably, leveraging used powders, machine turnings, and revert as feedstock. Through our UniMelt process, we transform these input streams into high-value AM powder, effectively converting scrap into a valuable resource. This innovative approach allows your organization to maximize the value of past powder investments by participating in 6K Additive’s powder buy-back program.

Nickel Ni625 Metal Powders Specifications

NOMINAL CHEMISTRY
Nickel Balance Silicon 0.50% (Max)
Chromium 20.0-23.0% Tantalum 0.40%
Molybdenum 8.00-10.00% Aluminum 0.40%
Iron 5.00% Carbon 0.10% (Max)
Niobium +Tantalum 3.15-4.15% Oxygen 0.03% (Max)
Cobalt 1.00% (Max) Nitrogen 0.02% (Max)
Copper 0.50% (Max) Phosphorous 0.015% (Max)
Manganese 0.50% (Max) Sulfur 0.015% (Max)
PHYSICAL PROPERTIES (Typical)
15-45 μm
Apparent Density 4.5 g/cm3
Tap Density 5.2 g/cm3
Hall Flow 17 x/50g
TENSILE PROPERTIES – Ni625
Powder YS (MPa) UTS (MPa) EL (%) RA (%)
XY 6K* 429 897 54 60
XY ASTM F3055* 275 485 30 30
Z 6K* 345 886 55 59
Z ASTM F3055* 275 485 30 30

*Annealed

Put our metal powders to the test

EXPORT CONTROLLED

Products, technical data, technology, and services of 6K Additive Products are subject to U.S. export controls under the Export Administration Regulations and the International Traffic in Arms Regulations. Products, data, and technology may not be resold, diverted, transferred, transshipped, made available to a foreign national within the United States, or otherwise disposed of in any other country outside of its intended destination, either in its original form or after being incorporated into other products or data without the prior written approval of 6K Additive. In addition, products, data, and technology may not be exported or re-exported to entities or persons that are ineligible under U.S. law to receive U.S. products and technology.