Nickel Superalloy Powder – Ni718

Nickel Ni718 Metal Powder For Additive Manufacturing

HIGH-PERFORMANCE PARTS START WITH HIGH-QUALITY NICKEL METAL POWDER

6K Additive nickel Ni718 metal powder for additive manufacturing. Ni718 is Ni-Cr-Mo-Ti precipitation hardening alloy with high-temperature strength and corrosion properties. 6K Additive’s Ni718 nickel metal powder properties make this alloy an attractive material for additive manufacturing applications where high-temperature oxidation is a concern such as aerospace, land-based turbine components, and other high-temperature industrial parts. Nickel alloy Ni718 has been a workhorse material for traditional AM components manufacturing and has quickly become a popular alloy for additive manufacturing.

Ni718 nickel metal powder is available in a variety of sizes. 6K Additive is a leading nickel metal powder manufacturer, so we can customize the PSD that you are looking for.

imgi_2_rocket-3d-print-metal

Ti6Al4V metal powder Printed Spinal Cage
Spinal cages designed and printed at Amplify Additive on a Trumpf TruPrint 1000 LPBF system with 6K Additive’s Ti6Al4V metal powder.

6K Additive Nickel Ni718 Metal Powder

6K’s UniMelt process is able to achieve industry-leading yields and obtain nickel Ni718 metal powders that perfectly match your desired particle size distribution (PSD) allowing for a variety of additive manufacturing processes when using nickel superalloy powder.

Ultra Clean
No Satellites
High Sphericity
Free Flowing
High Apparent Density
Low Porosity
Exceptional Lot-to-Lot Consistency
Conforms to AMS7006
Conforms to ASTM F3055
imgi_3_Ni718-Nickel-Superalloy-Powder

6K Additive Ni718 powder SEM

Industries & Applications for Nickel 718 Metal Powder

Ni718 powder is highly valued across a range of industries for its exceptional properties and versatile applications. With its outstanding properties, nickel alloy 718 has gained significant popularity in additive manufacturing, allowing for the production of intricate components in a wide range of crucial industries such as:

Aerospace
Land-Based Turbines
Industrial
Power Generation
Chemical Processing
Oil & Gas
imgi_4_Ni718-NICKEL-METAL-POWDER

6K Additive Ni718 powder SEM

Key Properties of Nickel Ni718 Metal Powder

Nickel superalloy powder Ni718 is highly valued across a range of industries for its exceptional properties and versatile applications. With its outstanding properties, nickel powder Ni718 has gained significant popularity in additive manufacturing, allowing for the production of intricate components in a wide range of crucial industries that use AM such as:

High-Temperature Strength
Superior Corrosion Resistance
Precipitation Hardening
Excellent Fatigue Resistance
Wide Operating Temperature Range
imgi_5_6k-Nickel-Life-Cycle-Assessment

LCA Nickel Life Cycle Assessment Report

Foresight Management completes the first-ever LCA for AM powder manufacturing processes for nickel powder production.

Sustainably Produced Nickel Metal Powder

At 6K Additive, our nickel powders are sourced sustainably, leveraging used powders, machine turnings and revert as feedstock. Through our UniMelt process, we transform these input streams into high-value AM powder, effectively converting scrap into a valuable resource. This innovative approach allows your organization to maximize the value of past powder investments by participating in 6K Additive’s powder buy-back program.

Nickel Ni718 Metal Powder Specifications

NOMINAL CHEMISTRY
Nickel 50.00-55.00% Carbon 0.08% (Max)
Chromium 17.00-21.00% Silicon 0.035% (Max)
Niobium +Tantalum 4.75-5.50% Nitrogen 0.03% (Max)
Molybdenum 2.80- 3.30% Oxygen 0.03% (Max)
Cobalt 1.00% (Max) Sulfur 0.015% (Max)
Titanium 0.65-1.15% Phosphorous 0.015% (Max)
Manganese 0.35% (Max) Boron 0.006% (Max)
Copper 0.30% (Max) Iron Balance
Aluminum 0.20-0.80%
PHYSICAL PROPERTIES (Typical)
15-45 μm
Apparent Density 4.5 g/cm3
Tap Density 5.2 g/cm3
Hall Flow 17 s/50g
TENSILE PROPERTIES – Ni718
Powder YS (MPa) UTS (MPa) EL (%)
XY 6K¹ 1227 1455 19
XY 6K² 1220 1413 23
XY ASTM F3055¹² 940 1240 12
Z 6K¹ 1241 1373 22
Z 6K² 1282 1413 24
Z ASTM F3055¹² 940 1240 12

¹ Solution & Dual-Age

²HIP, Solution & Dual Age

Put our metal powders to the test

EXPORT CONTROLLED

Products, technical data, technology, and services of 6K Additive Products are subject to U.S. export controls under the Export Administration Regulations and the International Traffic in Arms Regulations. Products, data, and technology may not be resold, diverted, transferred, transshipped, made available to a foreign national within the United States, or otherwise disposed of in any other country outside of its intended destination, either in its original form or after being incorporated into other products or data without the prior written approval of 6K Additive. In addition, products, data, and technology may not be exported or re-exported to entities or persons that are ineligible under U.S. law to receive U.S. products and technology.